The sanitary and stone cutting industry inevitably generates wastes. This study presents the use of quarry dust—a by-product of crushers as replacement of fine aggregate and ceramic waste as a replacement of coarse aggregate. The sources of ceramic waste are obtained from the industrial areas in Raipur. Presently, in ceramics industries the production goes as waste, which is not undergoing the recycle process yet. The potential of recycled ceramic waste as a substitute for coarse aggregates in concrete has been investigated. The recycling of ceramic waste has been done as it was used as aggregate. Concrete mix with 28 days characteristic strength of 20 MPa was prepared using water/cement ratio of 0.4. The study concludes that the 40% replacement of natural sand by quarry dust and 20% replacement of coarse aggregate by ceramic waste reveals higher strength as compared to 0% replacement of natural sand with quarry dust and 20% replacement of aggregate with ceramic waste. The concrete cubes were cast and tested for the destructive test at last which was compression test that to find out the compressive strength of specimens of hardened concrete at 7 days, 14 days and 28 days.
Die Inhaltsangabe kann sich auf eine andere Ausgabe dieses Titels beziehen.
EUR 3,40 für den Versand innerhalb von/der USA
Versandziele, Kosten & DauerAnbieter: Books Puddle, New York, NY, USA
Zustand: New. Bestandsnummer des Verkäufers 26395380586
Anzahl: 4 verfügbar
Anbieter: BuchWeltWeit Ludwig Meier e.K., Bergisch Gladbach, Deutschland
Taschenbuch. Zustand: Neu. This item is printed on demand - it takes 3-4 days longer - Neuware -The sanitary and stone cutting industry inevitably generates wastes. This study presents the use of quarry dust-a by-product of crushers as replacement of fine aggregate and ceramic waste as a replacement of coarse aggregate. The sources of ceramic waste are obtained from the industrial areas in Raipur. Presently, in ceramics industries the production goes as waste, which is not undergoing the recycle process yet. The potential of recycled ceramic waste as a substitute for coarse aggregates in concrete has been investigated. The recycling of ceramic waste has been done as it was used as aggregate. Concrete mix with 28 days characteristic strength of 20 MPa was prepared using water/cement ratio of 0.4. The study concludes that the 40% replacement of natural sand by quarry dust and 20% replacement of coarse aggregate by ceramic waste reveals higher strength as compared to 0% replacement of natural sand with quarry dust and 20% replacement of aggregate with ceramic waste. The concrete cubes were cast and tested for the destructive test at last which was compression test that to find out the compressive strength of specimens of hardened concrete at 7 days, 14 days and 28 days. 64 pp. Englisch. Bestandsnummer des Verkäufers 9786204190983
Anzahl: 2 verfügbar
Anbieter: Majestic Books, Hounslow, Vereinigtes Königreich
Zustand: New. Print on Demand. Bestandsnummer des Verkäufers 400996533
Anzahl: 4 verfügbar
Anbieter: Biblios, Frankfurt am main, HESSE, Deutschland
Zustand: New. PRINT ON DEMAND. Bestandsnummer des Verkäufers 18395380576
Anzahl: 4 verfügbar
Anbieter: moluna, Greven, Deutschland
Zustand: New. Dieser Artikel ist ein Print on Demand Artikel und wird nach Ihrer Bestellung fuer Sie gedruckt. Autor/Autorin: Manas DivyarthMy name is DIVYARTH MANAS. I am working as an Assistant Professor in Shri Shankaracharya Institute of Science and Technology from the past 4 years. Concrete technology my favorite work related area.The sanitary and . Bestandsnummer des Verkäufers 499981482
Anzahl: Mehr als 20 verfügbar
Anbieter: buchversandmimpf2000, Emtmannsberg, BAYE, Deutschland
Taschenbuch. Zustand: Neu. Neuware -The sanitary and stone cutting industry inevitably generates wastes. This study presents the use of quarry dust¿a by-product of crushers as replacement of fine aggregate and ceramic waste as a replacement of coarse aggregate. The sources of ceramic waste are obtained from the industrial areas in Raipur. Presently, in ceramics industries the production goes as waste, which is not undergoing the recycle process yet. The potential of recycled ceramic waste as a substitute for coarse aggregates in concrete has been investigated. The recycling of ceramic waste has been done as it was used as aggregate. Concrete mix with 28 days characteristic strength of 20 MPa was prepared using water/cement ratio of 0.4. The study concludes that the 40% replacement of natural sand by quarry dust and 20% replacement of coarse aggregate by ceramic waste reveals higher strength as compared to 0% replacement of natural sand with quarry dust and 20% replacement of aggregate with ceramic waste. The concrete cubes were cast and tested for the destructive test at last which was compression test that to find out the compressive strength of specimens of hardened concrete at 7 days, 14 days and 28 days.Books on Demand GmbH, Überseering 33, 22297 Hamburg 64 pp. Englisch. Bestandsnummer des Verkäufers 9786204190983
Anzahl: 2 verfügbar
Anbieter: AHA-BUCH GmbH, Einbeck, Deutschland
Taschenbuch. Zustand: Neu. nach der Bestellung gedruckt Neuware - Printed after ordering - The sanitary and stone cutting industry inevitably generates wastes. This study presents the use of quarry dust-a by-product of crushers as replacement of fine aggregate and ceramic waste as a replacement of coarse aggregate. The sources of ceramic waste are obtained from the industrial areas in Raipur. Presently, in ceramics industries the production goes as waste, which is not undergoing the recycle process yet. The potential of recycled ceramic waste as a substitute for coarse aggregates in concrete has been investigated. The recycling of ceramic waste has been done as it was used as aggregate. Concrete mix with 28 days characteristic strength of 20 MPa was prepared using water/cement ratio of 0.4. The study concludes that the 40% replacement of natural sand by quarry dust and 20% replacement of coarse aggregate by ceramic waste reveals higher strength as compared to 0% replacement of natural sand with quarry dust and 20% replacement of aggregate with ceramic waste. The concrete cubes were cast and tested for the destructive test at last which was compression test that to find out the compressive strength of specimens of hardened concrete at 7 days, 14 days and 28 days. Bestandsnummer des Verkäufers 9786204190983
Anzahl: 1 verfügbar