The samples were collected from the mountains of Malakand, KPK, and were grinded into smaller particles. The samples were extracted through the Soxhlet apparatus with different solvents to remove the soluble extractive and wax substances. The raw cellulose was treated in autoclave with alkaline substances for bond breaking. Most polar substances were removed through EDTA and hydrogen peroxide. Moreover, the samples were purified through acetic acid and nitric acid solution. The cellulose was neutralized by double distilled water until a neutral pH was obtained. The purified cellulose was characterized through different analytical techniques such as X-ray Diffraction (XRD) shows high crystallinity of 73%. FTIR shows the removal of different functional groups from the surface. TGA indicates that the cellulose obtained from different sources of wood showed that the loss of water takes place at 100οC, soluble extracted at 250οC, and lignin and hemicellulose at 350οC. SEM indicates that the surface morphology and shape are highly visible pores. The isolated cellulose has high crystallinity, thermal stability, and good mechanical properties.
Die Inhaltsangabe kann sich auf eine andere Ausgabe dieses Titels beziehen.
My name is Dr. Inamullah Mian. I have done my doctorate degree from the College of Chemistry and Chemical Engineering, Xinjiang University, (China) in 2020, under the Chinese government scholarship. Research expertise in the fields of thermal decomposition kinetics of biomass pellets and explained their reaction mechanism.
„Über diesen Titel“ kann sich auf eine andere Ausgabe dieses Titels beziehen.
Anbieter: Books Puddle, New York, NY, USA
Zustand: New. Bestandsnummer des Verkäufers 26395840871
Anzahl: 4 verfügbar
Anbieter: BuchWeltWeit Ludwig Meier e.K., Bergisch Gladbach, Deutschland
Taschenbuch. Zustand: Neu. This item is printed on demand - it takes 3-4 days longer - Neuware -The samples were collected from the mountains of Malakand, KPK, and were grinded into smaller particles. The samples were extracted through the Soxhlet apparatus with different solvents to remove the soluble extractive and wax substances. The raw cellulose was treated in autoclave with alkaline substances for bond breaking. Most polar substances were removed through EDTA and hydrogen peroxide. Moreover, the samples were purified through acetic acid and nitric acid solution. The cellulose was neutralized by double distilled water until a neutral pH was obtained. The purified cellulose was characterized through different analytical techniques such as X-ray Diffraction (XRD) shows high crystallinity of 73%. FTIR shows the removal of different functional groups from the surface. TGA indicates that the cellulose obtained from different sources of wood showed that the loss of water takes place at 100 C, soluble extracted at 250 C, and lignin and hemicellulose at 350 C. SEM indicates that the surface morphology and shape are highly visible pores. The isolated cellulose has high crystallinity, thermal stability, and good mechanical properties. 100 pp. Englisch. Bestandsnummer des Verkäufers 9786205489130
Anzahl: 2 verfügbar
Anbieter: Majestic Books, Hounslow, Vereinigtes Königreich
Zustand: New. Print on Demand. Bestandsnummer des Verkäufers 401584824
Anzahl: 4 verfügbar
Anbieter: Biblios, Frankfurt am main, HESSE, Deutschland
Zustand: New. PRINT ON DEMAND. Bestandsnummer des Verkäufers 18395840877
Anzahl: 4 verfügbar
Anbieter: moluna, Greven, Deutschland
Zustand: New. Dieser Artikel ist ein Print on Demand Artikel und wird nach Ihrer Bestellung fuer Sie gedruckt. The samples were collected from the mountains of Malakand, KPK, and were grinded into smaller particles. The samples were extracted through the Soxhlet apparatus with different solvents to remove the soluble extractive and wax substances. The raw cellulose . Bestandsnummer des Verkäufers 699354124
Anzahl: Mehr als 20 verfügbar
Anbieter: buchversandmimpf2000, Emtmannsberg, BAYE, Deutschland
Taschenbuch. Zustand: Neu. This item is printed on demand - Print on Demand Titel. Neuware -The samples were collected from the mountains of Malakand, KPK, and were grinded into smaller particles. The samples were extracted through the Soxhlet apparatus with different solvents to remove the soluble extractive and wax substances. The raw cellulose was treated in autoclave with alkaline substances for bond breaking. Most polar substances were removed through EDTA and hydrogen peroxide. Moreover, the samples were purified through acetic acid and nitric acid solution. The cellulose was neutralized by double distilled water until a neutral pH was obtained. The purified cellulose was characterized through different analytical techniques such as X-ray Diffraction (XRD) shows high crystallinity of 73%. FTIR shows the removal of different functional groups from the surface. TGA indicates that the cellulose obtained from different sources of wood showed that the loss of water takes place at 100¿C, soluble extracted at 250¿C, and lignin and hemicellulose at 350¿C. SEM indicates that the surface morphology and shape are highly visible pores. The isolated cellulose has high crystallinity, thermal stability, and good mechanical properties.VDM Verlag, Dudweiler Landstraße 99, 66123 Saarbrücken 100 pp. Englisch. Bestandsnummer des Verkäufers 9786205489130
Anzahl: 1 verfügbar
Anbieter: AHA-BUCH GmbH, Einbeck, Deutschland
Taschenbuch. Zustand: Neu. nach der Bestellung gedruckt Neuware - Printed after ordering - The samples were collected from the mountains of Malakand, KPK, and were grinded into smaller particles. The samples were extracted through the Soxhlet apparatus with different solvents to remove the soluble extractive and wax substances. The raw cellulose was treated in autoclave with alkaline substances for bond breaking. Most polar substances were removed through EDTA and hydrogen peroxide. Moreover, the samples were purified through acetic acid and nitric acid solution. The cellulose was neutralized by double distilled water until a neutral pH was obtained. The purified cellulose was characterized through different analytical techniques such as X-ray Diffraction (XRD) shows high crystallinity of 73%. FTIR shows the removal of different functional groups from the surface. TGA indicates that the cellulose obtained from different sources of wood showed that the loss of water takes place at 100 C, soluble extracted at 250 C, and lignin and hemicellulose at 350 C. SEM indicates that the surface morphology and shape are highly visible pores. The isolated cellulose has high crystallinity, thermal stability, and good mechanical properties. Bestandsnummer des Verkäufers 9786205489130
Anzahl: 1 verfügbar